Test Method Description
English
ASTM* C97 Absorption by weight: %   7.50
ASTM* C99 Modulus of rupture–dry specimens: psi 700.00
ASTM* C170 Compressive strength: psi   4,000.00
ASTM* C241 Abrasion resistance, hardness 6 min – 17 max
  Weight: lbs/cf   144.00
Most Indiana Limestone production possesses values higher than minimums listed here for engineering reference. Indiana Limestone is available with lower values. Consult ILI for particulars.